Conductor: Soft Annealed Tin Plated Copper, Stranded
Operating Temperature: 105°C
Operating Voltage: 600 Volts
Insulation: Extruded Layer of Cross-Linked Polyethlene
Reference: MIL-DTL-16878/36
Download pdf of this page
|
| |
Applications
This irradiation cross-linked polyethylene insulated wire is formulated to be fire resistant and produce low levels of smoke when burned. It meets the US Navy requirements for smoke, toxicity and acid gas. The insulation combines excellent thermal stability with very good wet electrical values. Having thermoset mechanical characteristics, it provides a superior small diameter, electronic hookup-wire.
|
Cable Specifications
| Type LS, 600 Volts |
|
| HP8LS-BDB-X |
26 |
.14 |
7/34 |
TC |
43.4 |
142 |
.041 |
1.04 |
1.50 |
2.23 |
| HP8LS-BEB-X |
24 |
.23 |
7/32 |
27.0 |
88.6 |
.046 |
1.17 |
2.10 |
3.13 |
| HP8LS-BFB-X |
22 |
.35 |
7/30 |
17.1 |
56.1 |
.052 |
1.32 |
3.10 |
4.61 |
| HP8LS-BGE-X |
20 |
.62 |
19/32 |
9.88 |
32.4 |
.060 |
1.52 |
4.70 |
6.99 |
| HP8LS-BHE-X |
18 |
.96 |
19/30 |
6.23 |
20.4 |
.070 |
1.78 |
7.10 |
10.6 |
| HP8LS-BJE-X |
16 |
1.23 |
19/29 |
4.81 |
15.8 |
.080 |
2.03 |
9.30 |
13.8 |
| HP8LS-BKE-X |
14 |
1.94 |
19/27 |
3.06 |
10.0 |
.096 |
2.44 |
14.1 |
21.0 |
| HP8LS-BLE-X |
12 |
3.08 |
19/25 |
1.92 |
6.30 |
.125 |
3.18 |
25.2 |
37.5 |
| HP8LS-BMG-X |
10 |
4.74 |
37/26 |
1.26 |
4.13 |
.155 |
3.94 |
38.7 |
57.6 |
| HP8LS-BNL-X |
8 |
8.61 |
133/29 |
.701 |
2.30 |
.225 |
5.72 |
65.0 |
96.7 |
| HP8LS-BPL-X |
6 |
13.6 |
133/27 |
.445 |
1.46 |
.265 |
6.73 |
101 |
150 |
| HP8LS-BRL-X |
4 |
22.0 |
133/25 |
.280 |
.919 |
.340 |
8.64 |
149 |
222 |
| HP8LS-BSP-X |
2 |
34.0 |
665/30 |
.183 |
.600 |
.420 |
10.7 |
237 |
353 |